The production and utilization of coal is based on well-proven and widely used technologies. Fly ash, a coal combustion byproduct, has potential to produce a composite material with controlled and superior properties. The major challenges with the production of fly ash are in its huge land coverage, adverse impact on environment etc. It puts pressure on the available land particularly in a densely populated country like India. In India the ash utilization percentage has not been very encouraging in spite of many attempts. Stabilization of fly ash is one of the methods to transfer the waste material into a safe construction material. This investigation is a step in that direction. This paper presents the results of an investigation on compressive strength and bearing ratio characteristics of surface coal mine overburden material and fly ash mixes stabilized with lime for coal mine haul road construction. Tests were performed with different percentages of lime (2, 3, 6 and 9%). The effects of lime content and curing period on the bearing ratio and tensile strength characteristics of the stabilized overburden and fly ash mixes are highlighted. Unconfined compressive strength test results cured for 7, 28 and 56 days are presented to develop correlation between different tensile strengths and unconfined compressive strength. Empirical models are developed to estimate bearing ratio and tensile strength of mine overburden–fly ash–quick lime mixtures from unconfined compressive strength test results.  相似文献   

2.
水泥土中掺入粉煤灰能在一定程度改善其性能,而变形特性是实际工程应用的重要指标。因此,研究粉煤灰和龄期对水泥土变形特性的影响对实际工程具有较大的参考价值。通过粉煤灰掺量为0和8%的水泥土无侧限抗压强度实验,研究发现养护龄期的增长与粉煤灰的掺加有利于水泥土变形模量的增长,尤其是粉煤灰的掺加有利于后期变形模量的增长。进一步对比分析两种粉煤灰掺量时的无侧限抗压强度和平均变形模量,发现它们之间基本上呈线性关系,随后通过拟合得出了它们之间的换算公式。最后,考虑应力-应变曲线模型特征以及对试验数据回归分析,推导出了一定条件下的水泥土应力-应变上升段表达式,为实际工程设计提供参考。  相似文献   

3.
粉煤灰与生石灰加固软土的室内试验研究   总被引:20,自引:5,他引:15  
林彤  刘祖德 《岩土力学》2003,24(6):1049-1052
粉煤灰是一种工业废弃物,与生石灰一样均可用来加固软土地基。笔者进行了粉煤灰与生石灰加固土的室内配方试验,分别将水泥或生石灰与粉煤灰按照不同的比例干拌均匀后,再与不同含水量的软土人工拌和均匀,测定了不同龄期的无侧限抗压强度;分析了石灰加固土强度与生石灰掺入比和龄期的关系及其压缩系数、压缩模量等的变化。并进一步分析了粉煤灰的加固机理,旨在为其进一步的研究和工程应用提供参考。  相似文献   

4.
为探究赤泥改性黄土的基本工程特性,进行无侧限抗压试验、直剪试验及渗透试验,得出赤泥改性黄土的最佳配比,建立了抗剪强度、无侧限抗压强度与电阻率的经验公式。通过动三轴试验,分析了循环动荷载下改性黄土的累积塑性变形、动弹性模量及浸出毒性。结果表明,随赤泥含量增加,改性黄土无侧限抗压强度和黏聚力都先增大后减小,当赤泥含量为15%时其28 d无侧限抗压强度达到3.5 MPa,较不掺入赤泥时提高约34.7%;改性黄土的渗透系数随赤泥含量增加先快速降低,至赤泥含量5%后趋于稳定;改性黄土的抗剪强度、无侧限抗压强度与电阻率呈良好的线性关系;改性黄土在循环动荷载下的临界动应力达600 kPa,最大动弹性模量比未改性黄土高出6倍,且其浸出液不具有浸出毒性。  相似文献   

5.
Hydro-mechanical evaluation of stabilized mine tailings   总被引:3,自引:0,他引:3  
. In this study, mine tailings waste was stabilized using a combination of lime, fly ash type "C", and aluminum. Treated samples were subjected to mineral identification for evaluating the formation of ettringite and gypsum. Also, unconfined compression, hydraulic conductivity, and cyclic freeze and thaw tests were performed to evaluate the hydro-mechanical properties of the stabilized samples. Experimental results have shown that the application of lime and fly ash type "C" to high sulfate content tailings has improved its plasticity, workability, and volume stability. Moreover, upon addition of aluminum to lime and fly ash in a sulfate-rich environment, ettringite and calcium sulfo-aluminate hydrate are formed in these samples. Application of 5% lime, 10% fly ash type "C", in combination with 110 ppm aluminum, resulted in the formation of a solid monolith capable of producing more than 1,000 kPa of unconfined compressive strength, and reduced tailings permeability to 1.96᎒–6 cm s–1, which is less than the recommended permeability of 10–5 cm s–1 by most environmental protection agencies for reusability of solidified/stabilized samples. The permeability of the treated tailings samples remained below the recommended permeability, even after exposing the treated samples to 12 freeze and thaw cycles. Therefore, based on the experimental results, it is concluded that treatment of high sulfate-content tailings with lime and fly ash, combined with the availability of aluminum for reactions, is a successful method of solidifying highly reactive mine tailings.  相似文献   

6.
查甫生  刘松玉  杜延军 《岩土力学》2006,27(Z1):549-554
研究掺粉煤灰对合肥膨胀土的物理性质指标以及胀缩性指标等的影响,探讨利用粉煤灰改良膨胀土的措施与效果。试验研究结果表明,在膨胀土中掺入适量的粉煤灰可有效降低膨胀土的塑性指数、降低膨胀势、减小线缩率与降低活性。在膨胀土中掺入粉煤灰还可改变膨胀土的击实特性,一定击实功作用下,随着掺灰率的增加,土体的最优含水率与最大干密度均减小,膨胀土中掺入粉煤灰后,膨胀土可在较小的含水率下通过击实或压实达到稳定。掺灰膨胀土的膨胀量与膨胀力随养护龄期的增长而减小;没有经过养护的掺灰土,其无侧限抗压强度随掺灰率的变化几乎没有变化,经过7 d养护后,土的无侧限抗压强度有所增长,并且存在一个峰值点,合肥膨胀土的无侧限抗压强度所对应的最佳掺粉煤灰率约为15 %~20 %。  相似文献   

7.
This paper presents the effects of addition of lime and lime along with gypsum on the compressibility behavior of two class F fly ashes. Since the fly ashes develop strength and exhibit lower compression, consolidation testing with conventional duration of load increment may not be appropriate. Hence, an attempt has been made to assess the minimum duration of load increment necessary to study the compressibility characteristics of such materials. Thus compressibility behavior of fly ashes with additives has been studied using conventional consolidation test with different durations of load increments varying from 30 min to 48 h. The results obtained indicated that 30 min of duration of load increment can be used to assess the compressibility behavior of such materials. The effect of lime which reduces the compression is seen to be maximum from the results obtained with the duration of load increment of 30 min but gradually reduces with higher durations of load increment. It has also been observed that the rate of decrease in the compressibility is maximum up to 2.5% lime and gradual thereafter. The compressibility of lime treated fly ashes further reduces when gypsum is incorporated, the optimum gypsum percentage being 2.5. This reduction in the compressibility of fly ashes enhanced by incorporating lime and gypsum makes them versatile in the construction of embankments and for structural fills, particularly reducing the time required in between laying of each lift.  相似文献   

8.
采用核磁共振技术,对不同配比的水玻璃、石灰+粉煤灰及石灰+粉煤灰+水玻璃的固化盐渍土的微观特征进行检测,结合无侧限抗压强度试验,分析了各固化方案的盐渍土固化效果,讨论了强度成因的微观特征机制。结果表明,不同固化土的孔隙特征有较大差异。石灰+粉煤灰固化盐渍土大孔隙减少;石灰+粉煤灰+水玻璃固化盐渍土孔隙总体积减少,但同时有大孔隙生成;水玻璃固化盐渍土孔隙总体增多,但随水玻璃浓度增大,孔隙体积有所减小。石灰+粉煤灰+水玻璃固化盐渍土抗压强度远大于其他固化方案,但是其孔隙结构并不是最优,说明颗粒间的胶结情况对固化效果的影响远大于孔隙特征。  相似文献   

9.
为研究石灰改性红砂岩残积土的工程性质并确定最佳掺量,以恩施地区红砂岩残积土为研究对象,制备不同石灰掺量的改良土试样,并进行击实、压缩、无侧限抗压试验。结果表明,随着石灰掺量的增大:改良土最优含水量逐渐增大,最大干密度逐渐减小;改良土压缩系数先减小后增大,压缩模量先增大后减小,对应的最优石灰掺量为7%;改良土无侧限抗压强度先提高后降低,对应的最优石灰掺量为9%。出现上述规律的主要原因是:石灰发生的水化、离子交换、碳酸化、结晶等作用,增强了砂土颗粒之间的黏结,提高了土的整体性,使石灰土压缩、强度特性得到改良。然而,过多的石灰会以自由灰的形式存在于土颗粒空隙之间,导致土体的压缩变形量增大,无侧限抗压强度降低。  相似文献   

10.
武汉东湖淤泥早强固化试验研究   总被引:5,自引:0,他引:5  
利用传统淤泥主固化材料水泥与辅助固化材料粉煤灰和石膏,通过组合配比对武汉东湖疏浚淤泥分别进行固化,基于无侧限抗压强度试验和三轴剪切试验,确定不同材料组合及配比下淤泥固化强度和特点。试验研究表明:在疏浚淤泥固化过程中水泥占主导地位,对固化效果影响最为显著;粉煤灰起到的作用相当于降低了淤泥初始含水率,表现在固化淤泥早期强度的快速提高;石膏有利于固化淤泥早期强度的形成,其作用持续于整个淤泥固化过程。随着含水率的增大,单纯水泥固化淤泥试样的应力-应变关系曲线由应变软化逐渐过渡到应变硬化模式,围压对固化淤泥强度的影响程度也随着含水率的增大而逐渐减弱,辅助固化材料的添加使原单纯水泥固化淤泥的应变硬化型曲线变为应变软化模式。不同含水率东湖疏浚淤泥固化材料最佳配比为水泥掺入比20%,粉煤灰为3倍的水泥量,石膏为30%的水泥量,该研究成果有助于武汉东湖底泥的治理以及疏浚淤泥排放场地的地基处理和环境整治。  相似文献   

11.
工业废渣加固土强度特性   总被引:3,自引:0,他引:3  
章定文  曹智国 《岩土力学》2013,34(Z1):54-59
工业废渣的资源化是解决工业废渣环境污染的有效途径之一。以粉煤灰和高炉矿渣为固化剂,石灰为碱性激发剂,对黏土进行加固。通过室内试验的方法,分析固化剂掺入量、养护龄期等对固化土无侧限抗压强度、pH值和饱和度等发展规律的影响。试验结果表明,固化土的无侧限抗压强度随固化剂掺入量的增加而增大,随养护龄期的增加而增大,提出一个综合反映固化剂掺入量、养护龄期和压实度等因素对固化土强度影响规律的综合影响因子,固化土强度与综合影响因子呈负指数函数关系;粉煤灰+石灰和高炉矿渣+石灰可有效改良土体无侧限抗压强度特性;石灰是一种有效的碱性激发剂,可提供工业废渣发生火山灰反应的高碱性环境。试验成果为工业废渣改良不良土质的设计提供试验依据。  相似文献   

12.
This study aims to express the relationships between Schmidt rebound number (N) with unconfined compressive strength (UCS) and Young's modulus (Et) of the gypsum by empirical equations. As known, the Schmidt hammer has been used worldwide as an index test for a quick rock strength and deformability characterisation due to its rapidity and easiness in execution, simplicity, portability, low cost and nondestructiveness. In this study, gypsum samples have been collected from various locations in the Miocene-aged gypsum of Sivas Basin and tested. The tests include the determination of Schmidt hammer rebound number (N), tangent Young's modulus (Et) and unconfined compressive strength. Finally, obtained parameters were correlated and regression equations were established among Schmidt hammer rebound hardness, tangent Young's modulus and unconfined compressive strength, presenting high coefficients of correlation. It appears that there is a possibility of estimating unconfined compressive strength and Young's modulus of gypsum, from their Schmidt hammer rebound number by using the proposed empirical relationships of UCS=exp(0.818+0.059N) and Et=exp(1.146+0.054N). However, the equations must be used only for the gypsum with an acceptable accuracy, especially at the preliminary stage of designing a structure. Finally, by using the obtained Schmidt hammer rebound number from this study, unconfined compressive strength was calculated and compared with the calculated value from different empirical equations proposed by different authors. It can be said that it is impossible to obtain only one relation for all types of the rocks.  相似文献   

13.
The effects of rate of strain on strength and deformation characteristics of soil–lime were investigated. Five strain rates (0.1, 0.8, 2.0, 4.0 and 7.0 %/min), five lime contents (0, 3, 6, 9 and 12 %) by dry soil weight and three cell pressures (100, 200 and 340 kN/m2) were carried. Triaxial tests, under unconsolidated condition, were used to study the effect of strain rate on strength and initial modulus of elasticity of soil and soil–lime mixture after two curing periods 7 and 21 days, respectively. A total of 405 triaxial specimens have been tested, where 225 specimens have been tested with first curing period (7 days). The testing program includes nine specimens for each strain rate, and each lime content was carried out, including natural soil with zero lime content. Another set of triaxial tests with a total of 180 specimens for the second curing period (21 days) was prepared at optimum moisture content, and the corresponding maximum dry density was also tested. The effects of strain rate and curing period on each of stress–strain behavior, type of failure, deviator stress at failure, cohesion and angle of internal friction and initial modulus of elasticity were studied thoroughly for the natural soil as well as soil–lime mixtures. For natural soil, the test results showed that the undrained shear strength, the initial modulus of elasticity and the cohesion increase significantly as the strain rate increase, while for soil–lime mixture at different curing periods, the undrained shear strength, initial modulus of elasticity and the cohesion increases to a maximum and then decreases as the strain rate and lime content increase. Also, the same variables and angle of internal friction increase with increasing curing period.  相似文献   

14.
水泥粉煤灰加固有机质土的试验研究   总被引:3,自引:0,他引:3  
对于高有机质含量的泻湖相软土,单纯采用水泥不能有效提高该软土的力学性能,因此提出了采用水泥和粉煤灰作为固化剂的加固方法。通过不同水泥掺入量、粉煤灰掺入量和龄期下水泥土的无侧限抗压强度试验,分析了水泥粉煤灰固化土的强度规律和变形规律,探讨了水泥和粉煤灰加固高有机质含量软土的机理。结果表明,粉煤灰对于水泥试块的早期强度影响较小,对后期强度影响较大;粉煤灰最佳掺入量为12%,超过此掺入量水泥土强度反而会降低,粉煤灰水泥土的破坏应变、E50也在粉煤灰掺量为12%时分别达到最低值和最大值。水泥掺加粉煤灰可有效地提高高有机质含量软土的强度。  相似文献   

15.
大掺量粉煤灰淤泥固化土的强度与耐久性研究   总被引:4,自引:0,他引:4  
王东星  徐卫亚 《岩土力学》2012,33(12):3659-3664
基于传统水泥和石灰固化处理方法,提出了利用大掺量低钙粉煤灰、水泥和石灰固化剂进行淤泥固化处理的方法,以期改善淤泥的强度和耐久性,达到淤泥和粉煤灰双重资源化利用的目的。通过一系列室内试验,探讨了该方法处理后固化淤泥的击实特征、强度特性、水稳性和耐久性。试验结果表明:淤泥固化后最优含水率有所降低、最大干密度则略有增加;弹性模量、无侧限抗压强度和抗拉强度均有不同程度的增加,水泥掺量越大,养护时间越长,强度和弹性模量越大;固化后淤泥水稳性得到明显改善;浸水软化和冻融循环导致固化土抗压强度显著劣化,冻胀融缩导致设计混合料的无侧限抗压强度减小约22%。  相似文献   

16.
聚苯乙烯轻质混合土的压缩变形特性试验研究   总被引:1,自引:0,他引:1  
聚苯乙烯轻质混合土是一种新型的填土材料,国内对其压缩变形特性的试验研究较少。在无侧限抗压强度试验基础上,分析了聚苯乙烯轻质混合土的破坏应变、变形系数与抗压强度的关系;依据单向固结压缩试验,分析了不同配比条件混合土的压缩变形特性,得到压缩屈服应力和压缩模量,可为工程应用提供参考依据  相似文献   

17.
Behavior of expansive soils stabilized with fly ash   总被引:6,自引:0,他引:6  
Expansive soils cause serious problem in the civil engineering practice due to swell and shrinkage upon wetting and drying. Disposal of fly ash, which is an industrial waste in both cost-effective and environment-friendly way receives high attention in China. In this study, the potential use and the effectiveness of expansive soils stabilization using fly ash and fly ash-lime as admixtures are evaluated. The test results show that the plasticity index, activity, free swell, swell potential, swelling pressure, and axial shrinkage percent decreased with an increase in fly ash or fly ash-lime content. With the increase of the curing time for the treated soil, the swell potential and swelling pressure decreased. Soils immediately treated with fly ash show no significant change in the unconfined compressive strength. However, after 7 days curing of the fly ash treated soils, the unconfined compressive strength increased significantly. The relationship between the plasticity index and swell-shrinkage properties for pre-treated and post-treated soils is discussed.  相似文献   

18.
Effect of Cement Type on the Mechanical Behavior of a Gravely Sand   总被引:1,自引:0,他引:1  
The behavior of a cemented gravely sand was studied using triaxial compression tests. Gypsum, Portland cement and lime were used as the cementing agents in sample preparation. The samples with different cement types were compared in equal cement contents. Three cement contents of 1.5%, 3.0% and 4.5% were selected for sample preparation. Drained and undrained triaxial compression tests were conducted in a range of confining pressures from 25 kPa to 500 kPa. Failure modes, shear strength, stress–strain behavior, volume and pore pressure changes were considered. The gypsum cement induced the highest brittleness in soil among three cement types while the Portland cement was found to be the most ductile cementing agent. In lower cement contents and lower confining pressures the soil cemented with Portland cement showed the highest shear strength. However, in the same range of cement content, the soil cemented with gypsum showed highest shear strength for highest tested confining stress. For higher cement contents the shear strength of soil cemented with Portland cement is higher than that for the two other cement types for the range of confining pressures tested in the present study. The samples cemented with lime had the least peak and ultimate shear strength and the highest pore pressure generation in undrained tests. Contrary to the soil cemented with lime, the brittleness of soil cemented with gypsum and Portland cement reduces in undrained condition. Finally it was found that the effect of cement type on the shear strength of cemented soils is more profound in drained condition compared to undrained state.  相似文献   

19.
The purpose of this paper is to investigate mechanical and hydraulic properties of sands treated with mineral-based grouts through the results of a laboratory test programme consisting of unconfined compression tests (UCS), triaxial bender element tests (BeT) and constant flow permeability tests in triaxial apparatus. An improved apparatus was set up for obtaining high quality, multiple grouted specimens from a single column. Two selected natural sands having different grain sizes were grouted with two mineral-based silica grouts, resulting in different levels of improvement. The behaviour of the sands treated by mineral grouts, in terms of strength, initial stiffness and permeability, was compared with that exhibited by more traditional silicate grouts. The results of this study indicate that sands treated with mineral grouts result in higher strengths, higher initial shear modulus and lower permeability values than the sands treated with the silicate solution. The effect of grout type, effective confining pressure, and sand particle-size on small-strain shear modulus of grouted sand specimens was evaluated. Based on test results, the small strain shear modulus increment from treated to untreated specimens has been correlated with the unconfined compressive strength, obtaining a unique relationship regardless of grout type and grain-size of tested sands.  相似文献   

20.
The use of fly ash in geotechnical engineering depends greatly on its pozzolanic reactivity. Though many factors influence the reactivity of fly ash it is well recognized that reactive silica and lime content play a major role. A new, accurate and reliable method for the determination of reactive silica content of fly ash has been established. The reactive silica content, obtained as acid soluble silica in about 2 to 3 N hydrochloric acid, is found to correlate well with unconfined compressive strength of fly ashes. The reactive silica content of fly ash is also important in the stabilization of soils using fly ash. © Rapid Science Ltd. 1998  相似文献   