1.
朱珍德  方荣  朱明礼  渠文平  阮怀宁 《岩土力学》2007,28(11):2279-2283
为了探讨温度周期变化与高围压对大理岩变形、强度特性及破坏断裂损伤劣化的影响,采用MTS815.03电液伺服刚性岩石试验系统,选取四川凉山雅砻江大河湾锦屏二级水电站引水隧洞围岩大理岩试样分别进行不同温度变化(100~ 600 ℃),周期次数为8次。进行高围压(60 MPa)作用下全应力应变过程三轴压缩与单轴压缩对比试验,系统分析比较了温度循环与高围压作用对大理岩应力-应变关系曲线、峰值应力、残余应力,峰值应变、残余应变以及弹性模量等的影响。试验结果表明,大理岩随着温度升高,峰值强度、残余强度、弹性模量下降,峰值应变和残余应变随之增大;在同一温度下,随着循环次数增加,其弹性模量、峰值强度、残余强度降低,温度越高,降低越明显;多次循环后,岩石的脆性变大,应力-应变曲线峰后段不再平滑,残余应变变小,其研究成果为锦屏二级水电站引水隧洞围岩稳定性分析提供理论依据。  相似文献   

2.
地下洞室开挖围岩经历典型径向卸载、环向加载应力路径,由此引起的岩体强度、变形特征和破坏机制也不尽相同。针对锦屏二级水电站高地应力赋存环境,对施工排水洞大理岩开展常规单轴全应变、三轴压缩、卸围压、卸围压-加载轴压等4种不同应力路径力学试验,得到应力-应变全过程曲线、变形破坏特征和极限储能变化规律。试验研究结果表明, (1)锦屏二级水电站大理岩破坏时轴向应变一般较小,为硬脆性材料,卸荷应力路径下该脆性特征更为明显;(2)卸围压同时加载轴压试验峰值强度对应轴向应变、环向应变及体积应变值一般高于单纯的卸围压值,而对应峰值强度则一般低于卸围压值;(3)卸荷速率较大时,变形模量越大,大理岩峰值强度越低。加载速率越大,变形模量越小,峰值强度越高。初始围压越高,变形模量值越低,峰值强度越高;(4)无侧限作用时试件主要为张拉破坏,低侧限作用时为剪切破坏为主,局部存在张拉破坏,较高侧限时,剪切面为典型X或Y型;(5)岩石试件具有极限储能值,该值受多种因素的影响。一般情况下试件破坏对应围压越高,极限储能值越高,卸载速率越大,极限储能值越小。研究结果对于岩爆孕育发生机制解释以及工程实际问题的解决均有参考价值。  相似文献   

3.
两种晶粒大理岩的力学性质研究   总被引:14,自引:1,他引:13  
尤明庆 《岩土力学》2005,26(1):91-96
矿物结构是影响岩石力学特性的根本因素。对晶粒0.5~1 mm细晶微风化大理岩和晶粒0.2~0.5 mm粉晶风化大理岩,进行了超声波测试和单轴、常规三轴压缩试验。粉晶大理岩晶粒尺度较小,滑移界面较多,粘接强度稍有变化就显著影响变形,即单轴压缩强度离散性较小而杨氏模量离散性较大,杨氏模量是细晶大理岩的1/3 左右,而单轴压缩强度仅低20 %。细晶大理岩的杨氏模量与围压无关,粉晶大理岩的杨氏模量随围压而增大,但进入延性变形阶段后两种大理岩的三轴强度完全相同。岩样的剪切破坏角都是随围压增大而减小,最后达到Coulomb准则确定的数值。在较高围压下,试样的承载极限与应力路径、材料强度以及内部的缺陷关系不大。晶粒的摩擦决定了大理岩的强度、变形特性。  相似文献   

4.
锦屏大理岩卸荷本构模型与数值模拟研究   总被引:1,自引:0,他引:1  
李新平  赵航  肖桃李 《岩土力学》2012,33(Z2):401-407
锦屏二级水电站深埋引水隧洞位于高地应力区,对取自隧洞内的大理岩进行常规三轴压缩试验、峰前卸围压试验。基于大理岩的峰前卸荷试验,研究峰前卸荷条件下岩石的变形、参数及破裂特征,建立峰前卸荷条件下岩石的幂函数型Mohr强度准则,给出数值仿真试验中大理岩的峰前卸载条件,利用有限差分程序FLAC3D建立了数值仿真模型,对模型进行了计算与分析,最后与室内试验结果对比,得到峰前卸荷状态下大理岩力学特性的相关规律。研究结果表明,幂函数型Mohr强度准则可较好地反映峰前卸荷条件下岩石的强度特性;卸围压初期,岩石试件呈现出明显的弹塑性特征;卸荷过程中岩石试件发生破坏时的峰值强度和围压降值随着围压增加而变大。研究结论揭示了锦屏大理岩卸载应力路径下的力学特性,具有一定的理论参考价值。  相似文献   

5.
岩石试样的强度准则及内摩擦系数   总被引:5,自引:1,他引:4  
岩石是一种非均质材料并含有各种缺陷,利用岩样的应力应交全程曲线可以确定理想强度,在排除岩样缺陷后讨论峰值强度与围压的关系,即强度准则。通过岩样剪切破坏后保持轴向变形恒定降低围压试验,可以确定岩样由摩擦力维持的承载能力随围压的变化关系。比较峰值强度和残余强度随围压变化关系的异同,可以研究岩样屈服过程中内摩擦系数的变化情况,以及内摩擦力对岩样变形特性的影响。粉砂岩试样在峰值应方时内摩擦系数已经达到最大值,峰后只是粘结力或者说是材料强度的降低过程,围压对变形没有明显影响。大理岩试样屈服过程中内摩擦系数不断增加,而内摩擦力的增加量与围压有关,高围压时只有材料强度完全丧失之后,由内摩擦力达到岩样的承载极限。内摩擦力系数随屈服过程增大,是岩石由脆性转交为廷性的根本原因。   相似文献   

6.
岩石抗压强度和变形参数是岩石工程设计的重要指标。由于岩石是典型的非均质材料,其强度和变形特性随样品尺 寸的变化而不同。本文采用PFC2D程序模拟了不同围压下不同尺寸岩样的压缩试验。结果表明(1) 岩样具有明显的尺寸效 应。同一围压下,尺寸越大,岩石强度、峰值应变和压缩模量越小,尺寸的变化对岩样的破坏模式影响较小;(2) 岩样具 有明显的围压效应。同一尺寸的岩样,随着围压的增大,岩石强度、峰值应变和压缩模量均增加,其中强度和峰值应变随 围压的增加呈线性增加。同时,随着围压的增大,岩石破裂模式由轴向劈裂破坏向剪切破坏变化;(3) 围压的存在会影响 岩样的尺寸效应。不同尺寸岩样的强度和峰值应变在相同围压区间内的增量基本相同,同时随着围压的增大,其强度和峰 值应变增加,进而使岩石强度和峰值应变的尺寸效应弱化;而不同尺寸岩样的压缩模量在相同围压区间内的增长率大致相 同,因而造成围压对压缩模量尺寸效应的影响较小  相似文献   

7.
《岩土力学》2017,(Z1):43-52
为揭示围压及应变速率对页岩力学特性的影响规律,对志留统龙马溪组页岩试样开展了不同围压及不同应变率下的三轴压缩力学试验研究。结果表明,围压和应变率对页岩的弹性模量、峰值强度及破裂形态等均具有显著影响,弹性模量和峰值强度均随围压的升高而增加,峰值强度增加的幅度明显大于弹性模量,峰值强度呈线性增加趋势,低围压时应变率从低到高,弹性模量和峰值强度都呈逐渐升高的趋势,两者与应变率对数的关系可用二次多项式描述;随着围压增大,页岩的应变率效应逐渐减弱,在较高高围压(50 MPa)下峰值强度和弹性模量随应变速率增加而增加现象均变得极不显著。对试验后岩样的破坏模式进行分析可知,页岩在低围压高应变率状态下主要是劈裂–剪切破坏,随着围压的增加和应变率的减小,试样的破坏由脆性劈裂–剪切破坏向单一剪切破坏转变,再逐渐向延性破坏过渡。研究结果对于合理确立页岩力学参数及设计压裂方案具有较好的参考。  相似文献   

8.
岩体经受自然冻融循环过程后,其物理力学性质的劣化是引起岩石工程灾害的主要原因。借助于MTS815液伺服岩石试验系统对经历不同冻融循环次数的粗砂岩进行三轴压缩试验,研究经历不同冻融循环次数后岩石在不同围压下的强度和变形特性,分析冻融循环次数和围压对岩石强度和变形的影响规律。研究结果表明,在冻融循环次数一定的条件下,随着围压的增加,岩石的三轴抗压强度、弹性模量和峰值轴向应变逐渐增加,表明粗砂岩的破坏逐渐由脆性破坏向塑形破坏变化;在围压相同的情况下,随着冻融循环次数的增加,岩石的三轴抗压强度、弹性模量逐渐减小,峰值应力对应的轴向应变逐渐增加;随着冻融循环次数的增加,粗砂岩的黏聚力均呈指数衰减形式降低,内摩擦角变化很小。   相似文献   

9.
峰后岩石剪胀性能试验研究   总被引:10,自引:0,他引:10  
靖洪文 《岩土力学》2003,24(1):93-96
采用美国MTS815型电液伺服岩石力学试验系统,对18块大理岩试件进行了试验,从6种不同围压下岩石应力-应变试验中,获得了岩石强度、剪胀力及体积应变随围压的变化情况规律,揭示了高应力松动、圈巷道围岩大变形的力学机理。提出了破裂岩体围岩与支护相互作用及最佳支护力位于“剪胀二期”初始点的新观点。  相似文献   

10.
刘亚洲  徐进  吴平  何伟 《岩矿测试》2009,28(5):483-487
对攀枝花钒钛磁铁矿尖山矿区的细粒和中粒辉长岩进行了单轴压缩、常规三轴压缩、抗拉强度和软化等系列岩石力学试验,研究了岩石结构(矿物颗粒大小)、水和围压等因素对岩石强度和变形特性的影响。结果表明,细粒辉长岩单轴抗压强度、弹性模量和压拉比均高于中粒辉长岩,但在三轴压缩情况下,两种岩石的峰值强度、残余强度和弹性模量差异较小;与中粒辉长岩相比,细粒辉长岩的峰值强度的黏聚力C较大,而峰值强度的内摩擦角φ较小;随着围压的增长,辉长岩峰值强度、残余强度与围压近似呈线性关系,剪切破坏角减小,平均模量E增长不明显,割线模量E50增长较显著;辉长岩的软化系数较高,在水的作用下弹性模量降低,泊松比升高。  相似文献   

11.
Fissures in natural rocks play an important role in determining the strength, deformability and failure behavior of rock mass. However in the past, triaxial compression experiments have rarely been conducted for rock materials containing three-dimensional (3-D) fissures and the failure mechanical behavior of fissured rocks is not well known due to the difficulty of conducting triaxial experiments on fissured rocks. Therefore in this research, conventional triaxial compression experiments were performed to study the strength, deformability and failure behavior of granite specimens with one preexisting open fissure. Thirty-one specimens were prepared to perform conventional triaxial compression tests for intact and fissured granite. First, based on the experimental results, the effects of the confining pressure and the fissure angle on the elastic modulus and the peak axial strain of granite specimens are analyzed. Second, the influence of the confining pressure on the crack damage threshold and the peak strength of granite with respect to various fissure angles are evaluated. For the same fissure angle, the crack damage threshold and the peak strength of granite both increase with the confining pressure, which is in good agreement with the linear Mohr–Coulomb criterion. With increasing fissure angle, the cohesion of granite first increases and later decreases, but the internal friction angle is not obviously dependent on the fissure angle. Third, nine crack types are identified to analyze the failure characteristics of granite specimens containing a single fissure under conventional triaxial compression. Finally, a series of X-ray microcomputed tomography (CT) observations were conducted to analyze the internal damage mechanism of granite specimens with respect to various fissure angles. Reconstructed 3-D CT images indicate obvious effects of confining pressure and fissure angle on the crack system of granite specimens. The study helps to elucidate the fundamental nature of rock failure under conventional triaxial compression.  相似文献   

12.
川藏铁路在穿越西藏贡觉地区时遇到三叠系粉砂质泥岩,在高地应力条件下容易发生大变形等危害。文章开展了不同围压下的岩石三轴压缩和和三轴蠕变试验,结合PFC数值模拟,研究了粉砂质泥岩在不同围压下的蠕变特性和长期强度研究,结果表明:贡觉粉砂质泥岩流变具有西原蠕变模型特征,蠕变与常规三轴试验条件下,随着围压不断增大,粉砂质泥岩试样均由拉-剪破坏向单剪破坏过渡,剪切破裂面与水平线的夹角逐渐减小,微裂纹数量减少;蠕变试验相较于常规三轴试验,由拉应力引起的压碎带影响范围更广;在高围压条件下,粉砂质泥岩更容易发生流变,随着围压的增大,轴向应变、侧向应变和体积应变均增大,微裂纹数量呈下降趋势;瞬时弹性模量及黏弹性系数与围压呈线性递增关系,黏弹性模量与围压呈对数型增长关系,黏塑性系数与围压呈指数型增长关系。在荷载长期作用下,岩石长期强度低于瞬时强度。  相似文献   

13.
硬石膏常规三轴压缩下强度和变形特性的试验研究   总被引:2,自引:1,他引:1  
郭印同  杨春和 《岩土力学》2010,31(6):1776-1780
采用伺服刚性试验机对硬石膏进行了不同围压下的常规三轴试验,研究了硬石膏的强度和变形特性。结果表明,在低围压下硬石膏破坏方式为剪切破坏;在围压超过10 MPa时,硬石膏表现出明显的塑性流动特性。观察试验后试样发现,在围压为18 MPa时,硬石膏已经没有明显的破坏面,而是表现出明显的膨胀现象。硬石膏的峰值强度与围压近似成正比例关系。分析了峰值应变、弹性模量随围压的变化规律,其结果表明:随着围压的升高,硬石膏的的峰值应变与弹性模量均逐渐增加。根据三轴试验结果绘制了摩尔包络线,采用回归分析得到了强度准则和抗剪强度参数c、? 值,其研究结果可为地下工程提供参考与借鉴。  相似文献   

14.
高温作用后花岗岩三轴压缩试验研究   总被引:2,自引:0,他引:2  
徐小丽  高峰  张志镇 《岩土力学》2014,35(11):3177-3183
为综合考察温度、围压对花岗岩力学性质及破坏方式的影响,在高温(25℃~1 000 ℃)作用后,利用MTS815.02电液伺服材料试验系统对花岗岩岩样进行不同围压作用下的三轴压缩试验。研究结果表明,(1)围压一定时,经历不同高温作用后花岗岩三轴压缩全应力-应变曲线经历了压密、弹性、屈服、破坏、塑性流动5个阶段;(2)经历不同高温作用后岩样三轴抗压强度与围压呈非线性二次多项式增长关系,围压为40 MPa时的抗压强度比单轴抗压强度提高了382.30%;常规三轴压缩条件下,400 ℃是花岗岩力学参数的阀值温度;(3)经历高温作用后,岩样弹性模量随围压升高呈增大趋势,围压为40 MPa时的弹性模量比单轴时提高了90.26%;随温度升高呈二次非线性减小,1 000 ℃时的弹性模量比25℃时降低了57.16%;(4)花岗岩的失稳型式同时取决于围压和温度。单轴压缩状态下,随着温度的升高,岩样变形破坏型式由脆性破裂向塑性变形过渡,失稳型式在低温时为突发失稳、中高温为准突发失稳,温度高于800 ℃为渐进破坏;三轴压缩状态下,随着围压的增大,岩样破裂型式由脆性张拉破裂逐渐向剪切破裂过渡,岩样的失稳型式以突发失稳为主。在试验温压范围内,影响花岗岩力学性质的首要因素是温度,其次是围压。  相似文献   

15.
基于残余强度修正的岩石损伤软化统计本构模型研究   总被引:3,自引:0,他引:3  
曹瑞琅  贺少辉  韦京  王芳 《岩土力学》2013,34(6):1652-1660
岩石随着围压的增大,残余强度的增加幅度比峰值强度大,残余强度逐渐成为影响岩石全应力-应变曲线峰后段的主要因素,因此,建立岩石损伤软化统计本构模型时,对残余强度进行修正是非常必要的。基于岩石应变强度理论以及岩石微元强度服从Weibull随机分布的假设,考虑岩石峰后残余强度对损伤变量进行修正,在微元破坏符合Hoek-Brown屈服准则条件下,建立了能够反映岩石峰后软化特征的三维损伤统计本构模型;依据岩石试验全应力-应变曲线的几何特征,推导出本构模型参数的数学表达式,并基于花岗岩室内试验数据对模型参数进行探讨,研究了Weibull分布参数与本构模型的关系,探讨了损伤修正系数的取值和岩石累积损伤的扩展过程;将建立的本构模型理论曲线与4种岩石(斑状二长花岗岩、细晶大理岩、砂岩和粉砂质泥岩)不同围压下的常规三轴压缩试验曲线进行对比分析,结果表明,该模型能很好地描述岩石破裂过程的全应力-应变关系和表征岩石残余强度特征。这对于岩石损伤软化问题以及岩石加固处理措施的研究均具有重要的意义。  相似文献   

16.
为准确地测量岩石试样在不同围压作用下的拉伸强度与变形特性,对用于岩石三轴压缩试验的MTS815材料试验机为主体设备进行了一系列技术改造,一方面设计加工了一套试验机活塞与三轴室的随动连锁装置,使原本只能提供压缩载荷的MTS815试验机也能精确提供轴向拉伸荷载;另一方面设计开发一种多自由度岩石试样三轴拉伸夹具,解决岩石等脆性材料在拉伸过程中难以始终保持对中的技术难题。提出一套完整的测试技术方法,能实现0~140 MPa围压范围内各种岩石试件的复杂三轴直接拉伸测试研究,利用研发的配套装置与测试方法对页岩试样进行了三轴拉伸试验。结果表明,试验装置和试验方法完全能够进行不同围压条件下的岩石三轴拉伸试验,得到相应的三轴拉伸试验曲线;页岩在低围压和高围压下呈现不同的破坏特征和破坏形式,低围压下依然呈现脆性特征,高围压下则是由脆性向塑性转换。  相似文献   