排序方式: 共有36条查询结果,搜索用时 15 毫秒
1.
2.
CAO Hong MA Enbao WANG Xuehua CHEN Jiazang BIN Xiaobei 《《地质学报》英文版》2006,80(2):285-289
By loading nanometer anatase onto exfoliated graphite with the sol-gel method, exfoliated graphite-TiO2 composite (EG-TiO2) can be prepared, which can adsorb oil and can also degrade oil. In a technologic condition for preparing EG-TiO2, the impregnated number of times is the most important factor to influence oil-adsorbing capability, that is, when the impregnated number of times increases, the amount of saturation-adsorbed oil decreases. The study of EG-TiO2 photocatalytic degradation of machine oil based on the weight-loss method and infrared spectrum method indicates that EG-TiO2 has obvious effect of photocatalytic degradation for machine oil. Its performance is superior to pure nanometer TiO2 powder because nanometer TiO2 in EG-TiO2 has three-dimension laminar structure and comparatively high adsorption capability. 相似文献
3.
纳米级微粒测量是寻找隐伏矿的新方法,选取实地模拟实验和在已知隐伏矿区,利用液态捕集剂和等离子体质谱分析测试样品,进行重复测量试验,研究结果表明,不同成矿元素,在地表形成异常的运移富集速率不同,其运移速率主要取决于纳米级微粒本身的地球化学性质,地下上升气流、断裂等裂隙有利于微粒的上升运移富集;纳米级微粒地球化学重复测量时,异常可具有良好的重现性,但异常重现较常规气体缓慢,通常需要2~3个月。 相似文献
4.
通过共沉淀法制备纳米Fe_2O_3-SnO_2光催化剂,采用XRD、SEM等测试手段对其进行形貌、物象、粒径一系列的表征,研究结果显示制得的催化剂仍保持纯SnO_2四方金红石型结构.研究了Fe_2O_3-SnO_2光催化剂投加量、Fe_2O_3与SnO_2物质的量比、煅烧温度、煅烧时间、氨氮初始浓度、p H值、H2O2浓度以及光照反应时间等因素对海水养殖废水中氨氮降解效率的影响.在紫外光照射下进行正交实验,确定最优化反应条件:催化剂投加量为0.4 g/dm3,煅烧时间为3 h,物质的量比为1∶2,氨氮初始含量为50 mg/dm3,光照反应时间为2 h.这5个因素对Fe_2O_3-SnO_2光催化氧化速率影响的大小程度依次为:Fe_2O_3与SnO_2物质的量比煅烧时间Fe_2O_3-SnO_2光催化剂投加量氨氮初始浓度光照时间.氨氮去除率可以达到85.1%,相同条件可见光下也可达到82.3%. 相似文献
5.
As the feature size of the CMOS integrated circuit continues to shrink, the more and more serious scattering effect has a serious impact on interconnection performance, such as delay and bandwidth. Based on the impact of the scattering effect on latency and bandwidth, this paper first presents the quality-factor model which optimises latency and bandwidth effectively with the consideration of the scattering effect. Then we obtain the analytical model of line width and spacing with application of curve-fitting method. The proposed model has been verified and compared based on the nano-scale CMOS technology. This optimisation model algorithm is simple and can be applied to the interconnection system optimal design of nano-scale integrated circuits. 相似文献
6.
通过溶胶-凝胶法,以CNTS-TiO2为前驱物制备了Li+掺杂CNTS-TiO2的纳米复合光催化剂(以下均称为Li+/CNTS-TiO2),采用X射线衍射(XRD)、扫描电镜(SEM)等测试手段对光催化剂进行表征,结果表明制得的催化剂为纳米材料且在TiO2的基础上增大了比表面积。利用掺杂量为3%的Li+掺杂CNTS-TiO2复合光催化剂(以下均称为3%Li+/CNTS-TiO2)光催化降解海洋柴油污染,在可见光条件下考察了Li+掺杂量、煅烧温度、光催化剂投加量、柴油初始质量浓度、光催化反应时间、H2O2质量浓度等条件对光催化实验的影响。进行正交实验,确定最优化工艺条件为:Li+掺杂量为3%,光催化剂的煅烧温度为600 ℃,3%Li+/CNTS-TiO2的投加量为0.1 g/L,降解柴油初始质量浓度为0.4 g/L,光催化反应时间为3 h,H2O2质量浓度为0.6 g/L,降解率可以达到95%以上。同时对此光催化剂进行应用试验,试验结果表明光催化剂去除效果优异,去除率可达91.87%。 相似文献
7.
建立了以纳米二氧化钛(TiO2)作为吸附剂填充微柱,电感耦合等离子体质谱(ICP-MS)法测试Cu^2+,Cd^2+,Pb^2+和Ni^2+离子的分析方法.考察了不同pH值、洗脱液浓度、样品流速、体积和外源干扰离子的影响,实验结果表明在pH值8~10范围内待测离子可被TiO2定量吸附,2.0molL^-1HNO3可将吸附在微柱上的待测物完全洗脱,优化条件下本方法对溶液中Cu^2+,Cd^2+,Ph^2+和M^2+离子检出限分别为:0.02,0.01,0.01,0.02μgL~,相对标准偏差小于2%(n=7),富集系数50倍.对水系沉积物标准物质(GBW07310)的测定值与标准值相一致,方法具有简便、快速,灵敏度高,重现性好的优点,可满足河口水体与沉积物样品中痕量金属元素定量分析的要求. 相似文献
8.
块金成因新见及其分级 总被引:6,自引:0,他引:6
本文描述了块金的形成新机制。在热液中呈金氢化物、金羰基化合物及纳料金粒子、纳米金合金粒子活化迁移。在表生条件下,金硫代硫酸盐配合物、金粒子、金合金粒子是金迁移的主要形式。块金是地质的、化学的、物理的、生物化学的综合作用的结果。按块金成因分为内生块金和次生块金。按单块块金质量分为4级。 相似文献
9.
采用无机盐溶胶-凝胶法制备了颗粒均匀的形态为针状的(Eu2+,Dy3+)SrAl2O4纳米粉体.通过TG-DTA分析和X射线衍射和扫描电镜分析方法,对样品进行了微观结构和表面形态的表征.研究了纳米(Eu2+,Dy3+)SrAl2O4粉体在不同烧结温度下固相反应过程和成相规律.实验结果表明,当样品的烧结温度为500 ℃时是单一的Sr(NO3)2晶相;750 ℃左右生成了Sr3Al2O6,并伴有少量SrAl2O4晶体;1 100 ℃是生成了结晶度良好的针状纳米(Eu2+,Dy3+)SrAl2O4粉体.通过计算,样品粉体晶粒平均为80~100 nm.该晶体粒度随烧结温度升高而逐渐变大. 相似文献
10.
森林沼泽区富含有机质样品中金的存在形式及对分析的影响 总被引:1,自引:4,他引:1
为探讨中国东北森林沼泽地区富含有机质样品中金偏低的原因,采用了王水溶矿法和四酸溶矿法的AAS分析来测定样品中的Au。用四酸溶矿法驱除硅胶,明显地提高金的测定值,特别是对含量大于10-9的样品,2种分析方法的差别更大。通过以上研究发现,在森林沼泽区的富含有机质样品中,金除以有机质结合形式存在于介质中,还可能以胶体或纳米形式存在于样品中,并被SiO2胶体所包裹,在高浓度有机酸的保护下,金能在水溶液中呈活动形式做长距离迁移;但用王水溶矿法不能测定出这种被SiO2胶体包裹形式的金。 相似文献