某萤石矿阶段磨矿阶段浮选工艺探讨
引用本文:祖述宇,郭文军,刘国英.某萤石矿阶段磨矿阶段浮选工艺探讨[J].地质找矿论丛,2013,28(4):646-650.
作者姓名:祖述宇  郭文军  刘国英
作者单位:中钢集团天津地质研究院,天津300181
摘    要:某萤石矿中萤石与石英密切共生.采用磨矿-浮选工艺流程进行选矿试验,虽然所得萤石精矿w(CaF2)达98%以上,但精矿中杂质w(SiO2)>1%.采用阶段磨矿阶段浮选工艺流程,获得了w(CaF2)=98.07%,w(SiO2) =0.77%的优质萤石精矿;粗精矿再磨使萤石充分单体解离,有助于降低浮选精矿中二氧化硅.

关 键 词:萤石矿  阶段磨矿阶段浮选  降低二氧化硅含量
收稿时间:2013/10/24 0:00:00

Discussion on stage grinding and stage floatation technology used in a fluorite deposit
ZU Shuyu,GUO Wenjun and LIU Guoying.Discussion on stage grinding and stage floatation technology used in a fluorite deposit[J].Contributions to Geology and Mineral Resources Research,2013,28(4):646-650.
Authors:ZU Shuyu  GUO Wenjun and LIU Guoying
Institution:(Sinosteel Tianjin Geological Academy, Tianjin 300181 ,China)
Abstract:In a fluorite deposit fluorite is closely associated with quartz. Test of grinding-floatation tech- nology showed CaF2 grade 〉98%. However the impurity of quartz in the concentrate is〉1%. Applica- tion of stage grinding and stage floatation technology results in CaF2 grade =98.07% ,SiO2 =0.77%. Re- grinding of the crude concentrate brings full liberation of fluorite and facilitates reduction of silica in the concentrate
Keywords:fluorite mine  stage flotation stage grinding  reduce the silica content